Good god, be core full with that.
Did you find any references to sputtering the coating. I would think this would give you a more even and more adhesive coating. Some chemical engineering labs at universities do that and would probably coat it for free. I know Dr. Viljoen at Nebraska-Lincoln has a setup for that. He usually sputters metal but I think a Teflon target would work the same.
Sent from mobile
> On Nov 3, 2014, at 10:09 AM, <cdelect at juno.com> <cdelect at juno.com> wrote:
>
> Coating the bulb with Teflon involves coating the inside with a Teflon
> liquid aqueous dispersion, letting it dry, and then curing it in an oven
> at 380 to 400 degrees C for around 30 minutes while circulating dry air
> through the bulb.
> A little bit intricate but doable. Main concern is getting the bulb
> surface absolutely clean before coating.
> A hydrofluoric acid rinse is a must!
>
> Cheers,
>
> Corby
>
> _______________________________________________
> time-nuts mailing list -- time-nuts at febo.com
> To unsubscribe, go to https://www.febo.com/cgi-bin/mailman/listinfo/time-nuts
> and follow the instructions there.
More information about the Time-nuts_lists.febo.com
mailing list