[time-nuts] Re: pulling some crystals

Bob kb8tq kb8tq at n1k.org
Fri Dec 15 13:38:54 UTC 2023


Hi

That’s not what you would want to use in an OCXO application if you want reasonable aging. Cold weld is what folks have been using for many decades. That’s what you are seeing with the glass bottoms …. Yes, they are more expensive.

Bob

> On Dec 13, 2023, at 5:12 AM, glenlist via time-nuts <time-nuts at lists.febo.com> wrote:
> 
> Hi Bob
> 
> from the MFR
> 
> "Crystals are in resistance weld packages with nitrogen + helium atmosphere, dew point below minus 80 deg.C, tested on He-leak detector".
> 
> Now, all the really good crystals I have here out of ovens look like glass on the bottom of the round cans.  Something different.
> 
> On 13/12/2023 1:44 am, Bob kb8tq wrote:
>> Hi
> _______________________________________________
> time-nuts mailing list -- time-nuts at lists.febo.com
> To unsubscribe send an email to time-nuts-leave at lists.febo.com




More information about the Time-nuts_lists.febo.com mailing list